alloy steel tube
"
Kaltbezogen/rollte das legierter Stahl-Rohr, das für Gang-Rad-Achswelle nahtlos ist
Seamless Cold Drawn Or Cold Rolled Alloy Steel Tubing 41Cr4 40Cr DIN1.7035 For Gear Wheel , Axle , Shaft Alloy Steel Tubes 41Cr4 40Cr DIN1.7035 Seamless Steel Tubes with alloy steel grade 41Cr440CrDIN1.7035 International equivalent: JIS: SCr440 ASTM: 5140 ISO: 41Cr4 41Cr4DIN1.7035: C:0.42 Si:0.25 Mn:0.70 Cr: 1.05 40Cr: C:0.37-0.44 Si:0.17-0.37 Mn:0.50-0.80 Cr:0.80-1.10 Seamless steel tubes with these steel grade could achieve good mechanical properites with quenching and
kaltbezogenes Rohr des legierten Stahl-20CrNiMo für Gang-Kurbelwellen ISO-TS Standard
Products Description: used for Gears Crankshafts Chinese Grade 20CrNiMo Cold Drawn Seamless Alloy Steel Tubes Quick Detail: Chemical Compositions: Steel Grade C Si Mn Cr Ni Mo P S Ti 20CrNiMo 0.17-0.23 0.17-0.37 0.60-0.95 0.40-0.70 0.35-0.75 0.20-0.30 ≤0.035 ≤0.035 - AISI8620 0.18-0.23 0.15-0.35 0.70-0.90 0.40-0.60 0.40-0.70 0.15-0.25 ≤0.035 ≤0.040 - AISI8620H 0.17-0.23 0.15-0.35 0.60-0.95 0.35-0.65 0.35-0.75 0.15-0.25 - - - 20CrMnTiH 0.17-0.23 0.17-0.37 0.80-1.15 1.00-1.35 -
nahtloses Rohr 6mm Ods legierten Stahl-4130 warm gewalzt mit Zertifikat ISO9001
Products Description TORICH Hot Rolled Seamless Alloy Steel Tubing 4130 / 4140 / 42CrMo Standard ASTM A519 SeamlessCarbonandAlloySteelMechanicalTubing Key Word Alloy Steel Tubing Material 4130,4340,42CrMo Size OD: 6-450mm; WT: 1-50mm; Length: max12000mm Production method Hot Rolled, Cold drawn, Cold Rolled Chemical Requirement Steel Grade C Mn P, max S, max Si Cr Mo SAE 4130 0.28-0.33% 0.40-0.60% 0.40% 0.40% 0.15-0.35% 0.80-1.10% 0.15-0.25% SAE4140 0.38-0.43% 0.75-1.00% 0.40%
Nahtloser und geschweißter Nickel-legierter Stahl wässern Schläuche Inconel 625
Inconel 625 Seamless and welded Nickel Alloy Steel Tube water tubing Type: Nickel alloy steel pipes Application: For Seawater components, Flare stacks, Aircraft ducting systems Technique: Cold-finished, hot-finished Size: OD 5-420mm WT 0.5-50mm LENGTH max12000mm Product Description Chemical Composition: Grade (UNS) C Si Mn P S Cr Ni Mo Al Other N06625 0.1 0.50 0.50 0.015 0.015 20.0-23.0 Bal. 8.0-10.0 0.4 Ti≤0.40; Nb:3.15-4.15 Mechanical proporties: Finish Condition Yield
Legierter Stahl-Schläuche ASTM A213 T11 T22, Kessel-Stahlrohr mit runder Form
Alloy steel T11 T22 with SA213 boiler steel tubes standard Alloy steel tube T11 T22 with SA213 boiler steel tubes standard T11: C: 0.05-0.15 Si: 0.50-1.0 Mn: 0.30-0.60 P: 0.025 S: 0.025 Cr: 1.0-1.5 Mo: 0.44-0.65 T22: C: 0.05-0.15 Si: 0.50 Mn: 0.30-0.60 P: 0.025 S: 0.025 Cr: 1.9-2.6 Mo: 0.87-1.13
Nahtlose legierter Stahl-Rohre ASTM A519 AISI 4130
ASTM A519 AISI4130 AISI4140 Seamless Alloy Steel Tubes Size range: O.D.: 6-350mm W.T.:1-50mm L: according to customer requirement Steel Grade and Chemical Compositions: Steel Grade and Chemical Compositions C Si Mn P≤ S≤ Cr Mo 4130 0.28-0.33 0.15-0.35 0.40-0.60 0.040 0.040 0.80-1.10 0.15-0.25 4140 0.38-0.43 0.15-0.35 0.75-1.00 0.040 0.040 0.80-1.10 0.15-0.25 Mechanical Properties: Mechanical Properties Grade condition Ultimat Yield Elongation Rockwell Strength Strength
Tragen Sie Kobalt der Umwelt-legierter Stahl-Rohr-Legierungs-6B - basierte PED-Bescheinigung
Wear Environment Alloy Steel Pipe Alloy 6B Cobalt - Based PED Certification Alloy Steel Pipe Alloy 6B cobalt-based alloy Alloy 6B is a cobalt-based alloy for wear environment, anti-seizure, anti-wear, anti-friction. It has a low coefficient of friction, which can make sliding contact and other metals and no wear in most cases. Even without lubricant, or cannot use lubricant applications, Alloy 6B minimizes scuffing and wear. Alloy 6 B wear-resisting performance is inherent,
Super legierter Stahl-Rohr-Aushärtungs-Legierung 41 für Motorteile
Super Alloy Steel Pipe Precipitation Hardening Alloy 41 For Engine Components Alloy Steel Pipe Alloy 41 precipitation hardening Nickel-Base Superalloy Alloy41 is a precipitation hardening Nickel-Base Superalloy, and it has higher tensile and lasting creep strength and good oxidation resistance within the temperature range of 650~950℃. Since the alloy of aluminum, titanium, molybdenum content is high, the ingot blooming is more difficult, but the material after deformation has
Säurebeständigkeits-legierter Stahl-Rohr Incoloy 825 ASTM B423 ASTM B829 ASTM B705
Alloy Steel Pipe Incoloy seamless steel pipe 825 Chemical composition: Ni %:38-46 Cr %:19.5-23.5 Fe:Remained. C%:0.025 Mn%:1.0 Si%:0.5 Cu%:1.5-3.0 Mo%:2.5-3.5 Al%:0.2 Ti%:0.6-1.2 P%:0.02 S%:0.01 Characteristic: Good resistance to stress corrosion cracking. Good resistance to pitting and crevice corrosion. Good resistance to oxidatiom and non-oxidizing acidic heat energy. At room temperature and temperatures up to 550℃ have the good mechanical properties. Have certified